Iron-on Instructions
Top Heat (such as an iron)
- Temperature: 340 F (170 C)
- Time: 55-60 seconds
- Pressure: Medium/Firm
- Cover Sheet: Teflon
Top and Bottom Heat (such as a heat press)
- Upper Temperature: 340 F (170 C)
- Lower Temperature: 320 F (160 C)
- Time: 30-40 seconds
- Pressure: Medium/Firm
- Cover Sheet: 1/8" (2.5cm) Silicone Pad
NOTE: Pre-heat garments for 5-10 seconds before applying the badge
Compatible Fabrics: Cotton, Cotton/Poly Blends, 100% Polyester, Fleece and Wool
Not Recommended for: Leather, Nylon and certail coated athletic mesh or safety garments